ChemicalResistance
ChemicalResistance.org

FEP and Aluminum Oxide: Chemical Resistance

Fluorinated ethylene propylene

Rating

Concentration20 °C50 °CRemark
solidAA

Material comparison at 20 °C

Aluminum Oxide: Material comparison at 20 °CFEP: A (highlighted); Aluminium: A; ECTFE/ETFE: A; EPDM: A; Viton (FPM): A; HDPE: A.Aluminium: AECTFE/ETFE: AEPDM: AFEP: AFEPViton (FPM): AHDPE: ALDPE: ANBR: ANylon (PA): APolycarbonate: APETG: APMP: AAcetal (POM): APP: APolystyrene: APolysulfone: APTFE: APVC Rigid: APVC Flexible: APVDF: ASAN: ASilicone: ASS 304: ASS 316: A
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

FEP shows very good resistance (A) to Aluminum Oxide at solid at 20 °C, meaning the material remains essentially unaffected by this chemical under standard laboratory test conditions. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Aluminum Oxide is commonly encountered in chemical storage and electroplating. FEP (Fluorinated ethylene propylene) is a fluoropolymer typically used for seals, gaskets, valve seats and lined equipment. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.

Practical recommendation

FEP can be used with confidence for Aluminum Oxide containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. This holds true at both 20 °C and 50 °C, giving a good safety margin for typical process environments.

Did you know?

Chemical resistance testing according to DIN and ISO standards typically evaluates weight change, dimensional change, and retention of tensile strength after immersion.

Materials rated A or B at 20 °C

Based on the row for solid, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, LDPE A, Nylon (PA) A, Acetal (POM) A, Polycarbonate A, PVC Flexible A, Polystyrene A, Polysulfone A, PETG A, PMP A, SAN A
Fluoropolymers
PTFE A, PVDF A, ECTFE/ETFE A
Elastomers
EPDM A, Viton (FPM) A, NBR A, Silicone A
Metals
SS 316 A, SS 304 A, Aluminium A

About FEP

FEP has nearly the chemical resistance of PTFE and can be melt-processed. Its service temperature, about 200 °C, is lower than that of PTFE.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.