Compatibility Rating

At 20°C (68°F)
A
Excellent
Excellent resistance - recommended for continuous use
At 50°C (122°F)
NR
No Data
No data available

Comparison Table — All Materials for Barium Hydroxide

Material20°C50°C
HDPEAA
LDPEAA
PPAA
PTFEAA
PVDFAC
FEPAA
ECTFE/ETFENRNR
EPDMANR
Viton (FPM)AA
NBRAA
SiliconeNRNR
SS 316AA
SS 304AA
AluminiumCC
PVC RigidAC
PVC FlexibleANR
PMPAA
PolystyreneNRNR
SANNRNR
PolycarbonateCC
PETGNRNR
Acetal (POM)BB
Nylon (PA)ANR
PolysulfoneNRNR

A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data

🌡️ Temperature Note

Good resistance at both 20°C and 50°C. Maximum service temperature for this material is 100°C — above this, degradation risk increases significantly.

🔄 Better Alternative?

Consider: PVDF or PTFE. View all materials for Barium Hydroxide →

FAQ

Is Nylon (PA) resistant to Barium Hydroxide?

Nylon (PA) has Excellent (A) resistance to Barium Hydroxide at 20°C. Excellent resistance - recommended for continuous use.

Can I store Barium Hydroxide in Nylon (PA) containers?

Yes, Nylon (PA) is rated A (Excellent) for Barium Hydroxide.

All Materials for Barium Hydroxide All Chemicals for Nylon (PA)