PP and Beeswax: Chemical Resistance

Polypropylene

Rating

Concentration20 °C50 °CRemark
concentration not statedAC

Material comparison at 20 °C

Beeswax: Material comparison at 20 °CPP: A (highlighted); Aluminium: A; ECTFE/ETFE: A; FEP: A; Viton (FPM): A; HDPE: A.Aluminium: AECTFE/ETFE: AFEP: AViton (FPM): AHDPE: ALDPE: ANylon (PA): APolycarbonate: APETG: AAcetal (POM): APP: APPPTFE: APVDF: ASS 304: ASS 316: ANBR: BEPDM: CPMP: –Polystyrene: –Polysulfone: –PVC Rigid: –PVC Flexible: –SAN: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

PP shows very good resistance (A) to Beeswax at 20 °C, meaning the material remains essentially unaffected by this chemical under standard laboratory test conditions. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Beeswax is commonly encountered in oil and gas and petrochemical processing. PP (Polypropylene) is a thermoplastic typically used for tanks, piping, containers and liners. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.

Practical recommendation

PP can be used with confidence for Beeswax containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. At elevated temperatures (50 °C), some reduction in resistance occurs, so periodic inspection is advisable for heated applications. Always verify performance under actual operating conditions before committing to a design.

Did you know?

In industrial practice, PP components exposed to Beeswax are typically inspected for swelling, discoloration, or loss of mechanical strength as early indicators of chemical attack.

Materials rated A or B at 20 °C

Thermoplastics
HDPE A, LDPE A, Nylon (PA) A, Acetal (POM) A, Polycarbonate A, PETG A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
Viton (FPM) A, NBR B
Metals
SS 316 A, SS 304 A, Aluminium A

About PP

Polypropylene resists most acids, alkalis and salt solutions. Concentrated oxidising acids, chlorinated solvents and aromatic hydrocarbons attack it, and it turns brittle below about 0 °C.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.