Compatibility Rating
At 20°C
Poor
Not recommended - significant degradation expected
At 50°C
Poor
Not recommended - significant degradation expected
Why is PP rated this way to Carbon Disulfide?
PP is not recommended for use with Carbon Disulfide. Significant degradation or failure is expected.
⚠️ When NOT to use PP
Avoid using Polypropylene with concentrated oxidizing acids, chlorinated solvents, and aromatic hydrocarbons. Becomes brittle below 0°C.
Comparison Table — All Materials for Carbon Disulfide
| Material | 20°C | 50°C |
|---|---|---|
| HDPE | D | D |
| LDPE | D | D |
| PP | D | D |
| PTFE | A | NR |
| PVDF | A | A |
| FEP | A | A |
| ECTFE/ETFE | A | C |
| EPDM | D | D |
| Viton (FPM) | A | NR |
| NBR | D | D |
| Silicone | NR | NR |
| SS 316 | A | A |
| SS 304 | A | A |
| Aluminium | A | A |
| PVC Rigid | D | D |
| PVC Flexible | D | D |
| PMP | D | D |
| Polystyrene | D | D |
| SAN | D | D |
| Polycarbonate | D | D |
| PETG | NR | NR |
| Acetal (POM) | B | NR |
| Nylon (PA) | C | NR |
| Polysulfone | D | D |
A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data
🌡️ Temperature Note
Maximum service temperature for this material is 100°C. Always verify compatibility at your specific operating conditions.
🔄 Better Alternative?
Consider: PVDF or PTFE for higher temperatures. View all materials for Carbon Disulfide →
FAQ
Is Polypropylene (PP) resistant to Carbon Disulfide?
Polypropylene (PP) has Poor (D) resistance to Carbon Disulfide at 20°C.
Can I store Carbon Disulfide in Polypropylene (PP)?
Caution - Polypropylene (PP) is rated D for Carbon Disulfide.