Chloroform Resistance of EPDM

Is EPDM compatible with Chloroform? See the chemical resistance rating below.

Compatibility Rating

At 20°C (68°F)
D
Poor
Not recommended - significant degradation expected
At 50°C (122°F)
D
Poor
Not recommended - significant degradation expected

Why is EPDM rated this way to Chloroform?

EPDM is not recommended for use with Chloroform. Significant degradation or failure is expected.

⚠️ When NOT to use EPDM

Avoid using EPDM Rubber with mineral oils, petroleum fuels, and aromatic solvents which cause swelling and degradation.

Comparison Table — All Materials for Chloroform

Material20°C50°C
HDPECD
LDPEDD
PPCD
PTFEAA
PVDFAA
FEPAA
ECTFE/ETFEBC
EPDMDD
Viton (FPM)CD
NBRDD
SiliconeNRNR
SS 316AA
SS 304AA
AluminiumCC
PVC RigidDD
PVC FlexibleDD
PMPDD
PolystyreneDD
SANDD
PolycarbonateDD
PETGDD
Acetal (POM)DD
Nylon (PA)CD
PolysulfoneDD

A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data

FAQ

Is EPDM resistant to Chloroform?

EPDM has Poor (D) resistance to Chloroform at 20°C. Not recommended - significant degradation expected.

Can I store Chloroform in EPDM containers?

Use caution - EPDM is rated D (Poor) for Chloroform.