Compatibility Rating
Why is EPDM resistant to Copper Vitriol Copper Sulfate?
EPDM shows excellent resistance to Copper Vitriol Copper Sulfate due to its saturated polymer backbone resisting degradation from water, steam, acids, and alkalis.
⚠️ When NOT to use EPDM
Avoid using EPDM Rubber with mineral oils, petroleum fuels, and aromatic solvents which cause swelling and degradation.
Comparison Table — All Materials for Copper Vitriol Copper Sulfate
| Material | 20°C | 50°C |
|---|---|---|
| HDPE | A | A |
| LDPE | A | A |
| PP | A | A |
| PTFE | A | A |
| PVDF | A | A |
| FEP | A | A |
| ECTFE/ETFE | A | A |
| EPDM | A | NR |
| Viton (FPM) | A | A |
| NBR | B | NR |
| Silicone | NR | NR |
| SS 316 | A | A |
| SS 304 | A | A |
| Aluminium | D | D |
| PVC Rigid | A | C |
| PVC Flexible | A | NR |
| PMP | A | NR |
| Polystyrene | A | A |
| SAN | A | A |
| Polycarbonate | A | NR |
| PETG | B | B |
| Acetal (POM) | A | NR |
| Nylon (PA) | A | NR |
| Polysulfone | A | NR |
A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data
🌡️ Temperature Note
Good resistance at both 20°C and 50°C. Maximum service temperature for this material is 120°C — above this, degradation risk increases significantly.
🔄 Better Alternative?
Consider: Viton for oils, PTFE for universal. View all materials for Copper Vitriol Copper Sulfate →
FAQ
Is EPDM resistant to Copper Vitriol Copper Sulfate?
EPDM has Excellent (A) resistance to Copper Vitriol Copper Sulfate at 20°C. Excellent resistance - recommended for continuous use.
Can I store Copper Vitriol Copper Sulfate in EPDM containers?
Yes, EPDM is rated A (Excellent) for Copper Vitriol Copper Sulfate.