PETG and Cyclohexanone: Chemical Resistance

Polyethylene terephthalate glycol (co-polyester)

Rating

Concentration20 °C50 °CRemark
technical gradeD*–

* estimated rating, given in the source without a temperature

Material comparison at 20 °C

Cyclohexanone: Material comparison at 20 °CPETG: D (highlighted); Aluminium: A; FEP: A; HDPE: A; Nylon (PA): A; Acetal (POM): A.Aluminium: AFEP: AHDPE: ANylon (PA): AAcetal (POM): APTFE: APVDF: ASS 304: ASS 316: APP: BLDPE: CPMP: CEPDM: DViton (FPM): DNBR: DPolycarbonate: DPETG: DPETGPolystyrene: DPolysulfone: DPVC Rigid: DPVC Flexible: DSAN: DECTFE/ETFE: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

PETG is not resistant (D) to Cyclohexanone at technical grade and should not be used in direct contact. The chemical is expected to cause rapid degradation, which can include dissolution, cracking, severe swelling, or complete structural failure of the material.

Application context

Cyclohexanone is commonly encountered in chemical synthesis and coatings and paints. PETG (Polyethylene terephthalate glycol (co-polyester)) is a thermoplastic typically used for tanks, piping, containers and liners. Since Cyclohexanone is flammable, material selection must also consider the risk of static charge buildup and the need for proper grounding in storage and transfer systems.

Practical recommendation

PETG is not recommended for use with Cyclohexanone. The D rating indicates that the material will suffer rapid and severe degradation, which may include cracking, dissolution, severe swelling, or complete structural failure. Using this combination risks equipment damage, leaks, and potential safety incidents. Consider using HDPE, Nylon (PA), Acetal (POM) instead, which are rated A for this chemical and offer reliable long-term performance.

Did you know?

Chemical resistance testing according to DIN and ISO standards typically evaluates weight change, dimensional change, and retention of tensile strength after immersion.

Materials rated A or B at 20 °C

Based on the row for technical grade, 20 °C.

Thermoplastics
HDPE A, PP B, Nylon (PA) A, Acetal (POM) A
Fluoropolymers
PTFE A, PVDF A, FEP A
Metals
SS 316 A, SS 304 A, Aluminium A

About PETG

PETG is a co-polyester for clear containers. Strong acids and alkalis and most organic solvents attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.