ChemicalResistance ChemicalResistance.org ← Search

Epichlorohydrin Resistance of NBR

Is NBR compatible with Epichlorohydrin? See the chemical resistance rating below.

Compatibility Rating

At 20°C (68°F)
D
Poor
Not recommended - significant degradation expected
At 50°C (122°F)
D
Poor
Not recommended - significant degradation expected

Why is NBR rated this way to Epichlorohydrin?

NBR is not recommended for use with Epichlorohydrin. Significant degradation or failure is expected.

⚠️ When NOT to use NBR

Avoid using Nitrile Rubber (Buna-N) with strong oxidizers, ketones, chlorinated solvents, and ozone. Not suitable for polar solvents.

Comparison Table — All Materials for Epichlorohydrin

Material20°C50°C
HDPEANR
LDPEANR
PPBB
PTFEANR
PVDFCC
FEPAA
ECTFE/ETFENRNR
EPDMCNR
Viton (FPM)DD
NBRDD
SiliconeNRNR
SS 316NRNR
SS 304NRNR
AluminiumCC
PVC RigidDD
PVC FlexibleDD
PMPDD
PolystyreneNRNR
SANNRNR
PolycarbonateDD
PETGNRNR
Acetal (POM)ANR
Nylon (PA)DD
PolysulfoneNRNR

A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data

🌡️ Temperature Note

Maximum service temperature for this material is 100°C. Always verify compatibility at your specific operating conditions.

🔄 Better Alternative?

Consider: Viton for wider chemical range. View all materials for Epichlorohydrin →

FAQ

Is NBR resistant to Epichlorohydrin?

NBR has Poor (D) resistance to Epichlorohydrin at 20°C. Not recommended - significant degradation expected.

Can I store Epichlorohydrin in NBR containers?

Use caution - NBR is rated D (Poor) for Epichlorohydrin.

All Materials for Epichlorohydrin All Chemicals for NBR