Nylon (PA) and Iodine Tincture: Chemical Resistance

Polyamide (nylon)

Rating

Concentration20 °C50 °CRemark
concentration not statedDD

Material comparison at 20 °C

Iodine Tincture: Material comparison at 20 °CNylon (PA): D (highlighted); Aluminium: A; ECTFE/ETFE: A; Viton (FPM): A; HDPE: A; LDPE: A.Aluminium: AECTFE/ETFE: AViton (FPM): AHDPE: ALDPE: APMP: AAcetal (POM): APP: APTFE: APVDF: ASS 316: AEPDM: BSS 304: BNBR: CPolycarbonate: CPolystyrene: CSAN: CNylon (PA): DPAPVC Rigid: DPVC Flexible: DFEP: –PETG: –Polysulfone: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Nylon (PA) is not resistant (D) to Iodine Tincture and should not be used in direct contact. The chemical is expected to cause rapid degradation, which can include dissolution, cracking, severe swelling, or complete structural failure of the material.

Application context

Iodine Tincture is commonly encountered in bleaching and chemical processing. Nylon (PA) (Polyamide (nylon)) is a thermoplastic typically used for tanks, piping, containers and liners. Since Iodine Tincture is flammable, material selection must also consider the risk of static charge buildup and the need for proper grounding in storage and transfer systems.

Practical recommendation

Nylon (PA) is not recommended for use with Iodine Tincture. The D rating indicates that the material will suffer rapid and severe degradation, which may include cracking, dissolution, severe swelling, or complete structural failure. Using this combination risks equipment damage, leaks, and potential safety incidents. Consider using HDPE, LDPE, PMP instead, which are rated A for this chemical and offer reliable long-term performance.

Did you know?

Chemical resistance testing according to DIN and ISO standards typically evaluates weight change, dimensional change, and retention of tensile strength after immersion.

Materials rated A or B at 20 °C

Thermoplastics
HDPE A, PP A, LDPE A, Acetal (POM) A, PMP A
Fluoropolymers
PTFE A, PVDF A, ECTFE/ETFE A
Elastomers
EPDM B, Viton (FPM) A
Metals
SS 316 A, SS 304 B, Aluminium A

About Nylon (PA)

Polyamide (nylon) resists fuels, oils and many solvents. Mineral acids, even dilute, and strong oxidisers attack it, and it absorbs water.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.