Aluminium

Rating

Concentration20 °C50 °CRemark
1-10 %CD
50 %DD
66 %DD
70 %DD
100 %AA

Material comparison at 20 °C

Nitric Acid: Material comparison at 20 °CAluminium: D (highlighted); ECTFE/ETFE: A; FEP: A; PTFE: A; PVDF: A; SS 304: A.ECTFE/ETFE: AFEP: APTFE: APVDF: ASS 304: ASS 316: AViton (FPM): BHDPE: BPMP: BLDPE: CPVC Rigid: CAluminium: DAlEPDM: DNBR: DNylon (PA): DPolycarbonate: DPETG: DAcetal (POM): DPP: DPolystyrene: DPolysulfone: DPVC Flexible: –SAN: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

The resistance of Aluminium to Nitric Acid is concentration-dependent. Across the 5 tested concentrations (1-10 %, 50 %, 66 %, 70 %, 100 %), the 20 °C rating ranges from A at lower concentrations to D at higher ones. This means engineers must verify which concentration their process actually involves before relying on a single rating. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Nitric Acid is commonly encountered in metal finishing and laboratory work. Aluminium (Aluminium) is a metal typically used for vessels, heat exchangers, fittings and structural components. Because Nitric Acid is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

Aluminium is not recommended for use with Nitric Acid. The D rating indicates that the material will suffer rapid and severe degradation, which may include cracking, dissolution, severe swelling, or complete structural failure. Using this combination risks equipment damage, leaks, and potential safety incidents. Consider using ECTFE/ETFE, FEP, PTFE instead, which are rated A for this chemical and offer reliable long-term performance.

Did you know?

Temperature is often the deciding factor when selecting materials for Nitric Acid: even materials rated A at 20 °C may lose performance at elevated temperatures.

Materials rated A or B at 20 °C

Based on the row for 70 %, 20 °C.

Thermoplastics
HDPE B, PMP B
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
Viton (FPM) B
Metals
SS 316 A, SS 304 A

About Aluminium

Aluminium relies on a thin oxide layer. Strong acids, strong alkalis and mercury compounds destroy that layer.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.