ChemicalResistance
ChemicalResistance.org

NBR and Nitric Acid: Chemical Resistance

Nitrile butadiene rubber

Rating

Concentration20 °C50 °CRemark
1-10 %DD
50 %DD
66 %DD
70 %DD
100 %DD

Material comparison at 20 °C

Nitric Acid: Material comparison at 20 °CNBR: D (highlighted); ECTFE/ETFE: A; FEP: A; PTFE: A; PVDF: A; SS 304: A.ECTFE/ETFE: AFEP: APTFE: APVDF: ASS 304: ASS 316: AViton (FPM): BHDPE: BPMP: BLDPE: CPVC Rigid: CAluminium: DEPDM: DNBR: DNBRNylon (PA): DPolycarbonate: DPETG: DAcetal (POM): DPP: DPolystyrene: DPolysulfone: DPVC Flexible: –SAN: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

NBR maintains a consistent rating of D across all 5 tested concentrations (1-10 %, 50 %, 66 %, 70 %, 100 %) of Nitric Acid at 20 °C. The fact that the rating does not change with concentration within the tested range simplifies material selection, though the boundary conditions beyond this range remain untested. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Nitric Acid is commonly encountered in surface cleaning and chemical processing. NBR (Nitrile butadiene rubber) is an elastomer typically used for seals, O-rings, hoses and flexible connections. Because Nitric Acid is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

NBR is not recommended for use with Nitric Acid. The D rating indicates that the material will suffer rapid and severe degradation, which may include cracking, dissolution, severe swelling, or complete structural failure. Using this combination risks equipment damage, leaks, and potential safety incidents. Consider using ECTFE/ETFE, FEP, PTFE instead, which are rated A for this chemical and offer reliable long-term performance.

Did you know?

When choosing between elastomers for Nitric Acid service, engineers consider not just the resistance rating but also factors such as permeation rate, creep resistance, and weldability.

Materials rated A or B at 20 °C

Based on the row for 70 %, 20 °C.

Thermoplastics
HDPE B, PMP B
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
Viton (FPM) B
Metals
SS 316 A, SS 304 A

About NBR

Nitrile rubber resists mineral oils and fuels. Ketones, esters, chlorinated solvents, strong oxidisers and ozone attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.