HDPE and Phenol: Chemical Resistance

High-density polyethylene

Rating

Concentration20 °C50 °CRemark
10 %AA
100 %BC

Material comparison at 20 °C

Phenol: Material comparison at 20 °CHDPE: B (highlighted); Aluminium: A; ECTFE/ETFE: A; FEP: A; PMP: A; PP: A.Aluminium: AECTFE/ETFE: AFEP: APMP: APP: APTFE: APVDF: ASS 304: ASS 316: AHDPE: BHDPEViton (FPM): CLDPE: CPolysulfone: CPVC Flexible: CEPDM: DNBR: DNylon (PA): DPolycarbonate: DPETG: DAcetal (POM): DPolystyrene: DPVC Rigid: DSAN: DSilicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

The resistance of HDPE to Phenol is concentration-dependent. Across the 2 tested concentrations (10 %, 100 %), the 20 °C rating ranges from A at lower concentrations to C at higher ones. This means engineers must verify which concentration their process actually involves before relying on a single rating. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Phenol is commonly encountered in chemical synthesis and cosmetics production. HDPE (High-density polyethylene) is a thermoplastic typically used for tanks, piping, containers and liners. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.

Practical recommendation

HDPE is suitable for use with Phenol under normal conditions, but some minor effects on the material are expected over time. Periodic monitoring for swelling, softening, or weight change is recommended, especially for long-service components. Avoid prolonged exposure at elevated temperatures, as the resistance decreases further at 50 °C. For safety-critical or long-life applications, consider PMP, PP, ECTFE/ETFE instead, which are rated A for this chemical.

Did you know?

Chemical resistance testing according to DIN and ISO standards typically evaluates weight change, dimensional change, and retention of tensile strength after immersion.

Materials rated A or B at 20 °C

Based on the row for 100 %, 20 °C.

Thermoplastics
PP A, PMP A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Metals
SS 316 A, SS 304 A, Aluminium A

About HDPE

High-density polyethylene resists most aqueous acids, alkalis and salt solutions. Strong oxidising acids, chlorinated solvents and aromatic hydrocarbons attack or swell it. Continuous service is usually limited to about 80 °C.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.