Rating
| Concentration | 20 °C | 50 °C | Remark |
|---|---|---|---|
| aqueous | C | – | |
| saturated | D | D |
Material comparison at 20 °C
Resistance overview
The resistance of Nylon (PA) to Potassium Dichromate is concentration-dependent. Across the 2 tested concentrations (aqueous, saturated), the 20 °C rating ranges from C at lower concentrations to D at higher ones. This means engineers must verify which concentration their process actually involves before relying on a single rating. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.
Application context
Potassium Dichromate is commonly encountered in chemical processing and waste treatment. Nylon (PA) (Polyamide (nylon)) is a thermoplastic typically used for tanks, piping, containers and liners. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.
Practical recommendation
Nylon (PA) is not recommended for use with Potassium Dichromate. The D rating indicates that the material will suffer rapid and severe degradation, which may include cracking, dissolution, severe swelling, or complete structural failure. Using this combination risks equipment damage, leaks, and potential safety incidents. Consider using HDPE, LDPE, PMP instead, which are rated A for this chemical and offer reliable long-term performance.
Did you know?
The ratings shown here apply to pure Potassium Dichromate in contact with the base thermoplastic. In real-world applications, additives, pigments, and fillers in the material can shift resistance in either direction.
Materials rated A or B at 20 °C
Based on the row for saturated, 20 °C.
- Thermoplastics
- HDPE A, PP A, PVC Rigid A, LDPE A, PVC Flexible A, Polystyrene A, PMP A, SAN A
- Fluoropolymers
- PTFE A, PVDF A, FEP A
- Elastomers
- EPDM A, Viton (FPM) B
- Metals
- SS 316 A, SS 304 A, Aluminium A
About Nylon (PA)
Polyamide (nylon) resists fuels, oils and many solvents. Mineral acids, even dilute, and strong oxidisers attack it, and it absorbs water.
Rating scale
- A very good resistance
- B good resistance
- C limited resistance
- D not resistant
- – no data
- K no general statement possible
A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.
About this data
The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.
A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.