Compatibility Rating
At 20°C
Poor
Not recommended - significant degradation expected
At 50°C
Poor
Not recommended - significant degradation expected
Why is NBR rated this way to Potassium Permanganate?
NBR is not recommended for use with Potassium Permanganate. Significant degradation or failure is expected.
⚠️ When NOT to use NBR
Avoid using Nitrile Rubber (Buna-N) with strong oxidizers, ketones, chlorinated solvents, and ozone. Not suitable for polar solvents.
Comparison Table — All Materials for Potassium Permanganate
| Material | 20°C | 50°C |
|---|---|---|
| HDPE | A | C |
| LDPE | A | A |
| PP | A | A |
| PTFE | A | A |
| PVDF | A | A |
| FEP | A | A |
| ECTFE/ETFE | A | A |
| EPDM | A | NR |
| Viton (FPM) | A | A |
| NBR | D | D |
| Silicone | NR | NR |
| SS 316 | A | A |
| SS 304 | A | A |
| Aluminium | A | A |
| PVC Rigid | A | C |
| PVC Flexible | NR | NR |
| PMP | A | A |
| Polystyrene | A | C |
| SAN | A | C |
| Polycarbonate | A | NR |
| PETG | B | B |
| Acetal (POM) | A | A |
| Nylon (PA) | D | D |
| Polysulfone | NR | NR |
A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data
🌡️ Temperature Note
Maximum service temperature for this material is 100°C. Always verify compatibility at your specific operating conditions.
🔄 Better Alternative?
Consider: Viton for wider chemical range. View all materials for Potassium Permanganate →
FAQ
Is NBR resistant to Potassium Permanganate?
NBR has Poor (D) resistance to Potassium Permanganate at 20°C.
Can I store Potassium Permanganate in NBR?
Caution - NBR is rated D for Potassium Permanganate.