Aluminium and Sodium Bisulfate: Chemical Resistance

Aluminium

Rating

Concentration20 °C50 °CRemark
10 %AC
any concentrationAC

Material comparison at 20 °C

Sodium Bisulfate: Material comparison at 20 °CAluminium: A (highlighted); ECTFE/ETFE: A; EPDM: A; FEP: A; Viton (FPM): A; HDPE: A.Aluminium: AAlECTFE/ETFE: AEPDM: AFEP: AViton (FPM): AHDPE: ALDPE: ANBR: APolycarbonate: APETG: APP: APTFE: APVC Rigid: APVDF: ASS 304: ASS 316: AAcetal (POM): BNylon (PA): DPMP: –Polystyrene: –Polysulfone: –PVC Flexible: –SAN: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Aluminium shows excellent resistance to Sodium Bisulfate across all 2 tested concentrations (10 %, any concentration) at 20 °C, making it a reliable choice for storage, transfer, and handling applications involving this chemical at any of the tested strengths. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Sodium Bisulfate is commonly encountered in water treatment and food processing. Aluminium (Aluminium) is a metal typically used for vessels, heat exchangers, fittings and structural components. Because Sodium Bisulfate is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

Aluminium can be used with confidence for Sodium Bisulfate containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. At elevated temperatures (50 °C), some reduction in resistance occurs, so periodic inspection is advisable for heated applications. Always verify performance under actual operating conditions before committing to a design.

Did you know?

Chemical resistance testing according to DIN and ISO standards typically evaluates weight change, dimensional change, and retention of tensile strength after immersion.

Materials rated A or B at 20 °C

Based on the row for 10 %, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, LDPE A, Acetal (POM) B, Polycarbonate A, PETG A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A, Viton (FPM) A, NBR A
Metals
SS 316 A, SS 304 A

About Aluminium

Aluminium relies on a thin oxide layer. Strong acids, strong alkalis and mercury compounds destroy that layer.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.