ChemicalResistance
ChemicalResistance.org

PMP and Acetaldehyde: Chemical Resistance

Polymethylpentene (TPX)

Rating

Concentration20 °C50 °CRemark
40 %BD
technical gradeBD

Material comparison at 20 °C

Acetaldehyde: Material comparison at 20 °CPMP: B (highlighted); Aluminium: A; FEP: A; PTFE: A; SS 304: A; SS 316: A.Aluminium: AFEP: APTFE: ASS 304: ASS 316: AECTFE/ETFE: BLDPE: BNylon (PA): BPMP: BPMPAcetal (POM): BEPDM: CHDPE: CPP: CViton (FPM): DNBR: DPolycarbonate: DPETG: DPolystyrene: DPolysulfone: DPVC Rigid: DPVDF: DSAN: DPVC Flexible: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

PMP maintains a consistent rating of B across all 2 tested concentrations (40 %, technical grade) of Acetaldehyde at 20 °C. The fact that the rating does not change with concentration within the tested range simplifies material selection, though the boundary conditions beyond this range remain untested. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Acetaldehyde is commonly encountered in pharmaceutical manufacturing and electronics cleaning. PMP (Polymethylpentene (TPX)) is a thermoplastic typically used for tanks, piping, containers and liners. Since Acetaldehyde is flammable, material selection must also consider the risk of static charge buildup and the need for proper grounding in storage and transfer systems.

Practical recommendation

PMP is suitable for use with Acetaldehyde under normal conditions, but some minor effects on the material are expected over time. Periodic monitoring for swelling, softening, or weight change is recommended, especially for long-service components. Avoid prolonged exposure at elevated temperatures, as the resistance decreases further at 50 °C. For safety-critical or long-life applications, consider FEP, PTFE, Aluminium instead, which are rated A for this chemical.

Did you know?

Polymethylpentene (TPX) was first developed in the 1960s and remains one of the most widely used thermoplastics in chemical handling equipment.

Materials rated A or B at 20 °C

Based on the row for 40 %, 20 °C.

Thermoplastics
LDPE B, Nylon (PA) B, Acetal (POM) B
Fluoropolymers
PTFE A, FEP A, ECTFE/ETFE B
Metals
SS 316 A, SS 304 A, Aluminium A

About PMP

Polymethylpentene (TPX) is a transparent polyolefin used for labware. It resists many acids and alkalis, while aromatic and chlorinated solvents and strong oxidisers attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.