Aluminium

Rating

Concentration20 °C50 °CRemark
aqueousCD
solidCD

Material comparison at 20 °C

Ammonium Chloride: Material comparison at 20 °CAluminium: C (highlighted); ECTFE/ETFE: A; EPDM: A; FEP: A; Viton (FPM): A; HDPE: A.ECTFE/ETFE: AEPDM: AFEP: AViton (FPM): AHDPE: ALDPE: ANBR: ANylon (PA): APolycarbonate: APMP: APP: APolystyrene: APolysulfone: APTFE: APVC Rigid: APVC Flexible: APVDF: ASAN: ASS 304: ASS 316: APETG: BAcetal (POM): BAluminium: CAlSilicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Aluminium maintains a consistent rating of C across all 2 tested concentrations (aqueous, solid) of Ammonium Chloride at 20 °C. The fact that the rating does not change with concentration within the tested range simplifies material selection, though the boundary conditions beyond this range remain untested. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Ammonium Chloride is commonly encountered in waste treatment and bleaching. Aluminium (Aluminium) is a metal typically used for vessels, heat exchangers, fittings and structural components. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.

Practical recommendation

Aluminium has limited resistance to Ammonium Chloride and should only be used for short-term or intermittent contact at ambient temperature. The C rating means the material undergoes noticeable changes — swelling, loss of strength, or surface degradation — that make it unsuitable for permanent installations. For prolonged or continuous exposure, HDPE, LDPE, Nylon (PA) offer significantly better resistance and are rated A.

Did you know?

Chemical resistance testing according to DIN and ISO standards typically evaluates weight change, dimensional change, and retention of tensile strength after immersion.

Materials rated A or B at 20 °C

Based on the row for aqueous, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, LDPE A, Nylon (PA) A, Acetal (POM) B, Polycarbonate A, PVC Flexible A, Polystyrene A, Polysulfone A, PETG B, PMP A, SAN A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A, Viton (FPM) A, NBR A
Metals
SS 316 A, SS 304 A

About Aluminium

Aluminium relies on a thin oxide layer. Strong acids, strong alkalis and mercury compounds destroy that layer.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.