Comparison Table — All Materials for Ammonium Nitrate
| Material | 20°C | 50°C |
|---|---|---|
| HDPE | A | C |
| LDPE | A | A |
| PP | A | A |
| PTFE | A | A |
| PVDF | A | A |
| FEP | A | A |
| ECTFE/ETFE | A | A |
| EPDM | A | NR |
| Viton (FPM) | B | B |
| NBR | A | A |
| Silicone | NR | NR |
| SS 316 | A | A |
| SS 304 | A | A |
| Aluminium | B | B |
| PVC Rigid | A | A |
| PVC Flexible | A | NR |
| PMP | A | A |
| Polystyrene | A | NR |
| SAN | A | A |
| Polycarbonate | A | NR |
| PETG | B | B |
| Acetal (POM) | B | D |
| Nylon (PA) | A | NR |
| Polysulfone | A | NR |
A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data
🌡️ Temperature Note
Performance degrades significantly at higher temperatures — rated Excellent at 20°C but only Fair at 50°C. For elevated temperatures, consider a more resistant material. Max service temp: 80°C.
🔄 Better Alternative?
Consider: PP (higher temp) or PTFE (universal). View all materials for Ammonium Nitrate →
FAQ
Is HDPE resistant to Ammonium Nitrate?
HDPE has Excellent (A) resistance to Ammonium Nitrate at 20°C.
Can I store Ammonium Nitrate in HDPE?
Yes, HDPE is rated A for Ammonium Nitrate.