ChemicalResistance
ChemicalResistance.org

Ammonium Nitrate Chemical Resistance

Resistance ratings for 24 plastics, elastomers and metals at 20 °C and 50 °C. Listed at 2 concentrations, because the rating depends on it.

At a glance

Based on the row for 10 %, 20 °C.

Rated A, very good resistance
PTFE, HDPE, PP, PVDF, PVC Rigid, EPDM, NBR, SS 316, SS 304, Aluminium, FEP, ECTFE/ETFE, Nylon (PA), Polycarbonate, Polystyrene, Polysulfone (16)
Rated B, good resistance
Viton (FPM), Acetal (POM), PETG (3)
Rated C, limited resistance
none (0)
Rated D, not resistant
none (0)
No data in the source
LDPE, Silicone, PVC Flexible, PMP, SAN
Rated lower at 50 °C than at 20 °C
HDPE (A → C), PVC Rigid (A → C), Acetal (POM) (B → D)
Rating changes with concentration (20 °C)
Aluminium: A (10 %), B (saturated)

Based on the row for 10 %, 20 °C.

Rating profile by material family

Ammonium Nitrate: Rating profile by material familyThermoplastics: 7 A, 2 B, 4 no data. Fluoropolymers: 4 A. Elastomers: 2 A, 1 B, 1 no data. Metals: 3 A.Thermoplastics (13)Thermoplastics: 7 × A, very good resistance (HDPE, PP, PVC Rigid, Polystyrene, Polycarbonate, Nylon (PA), Polysulfone)A 7Thermoplastics: 2 × B, good resistance (PETG, Acetal (POM))B 2Thermoplastics: 4 × no data (LDPE, PVC Flexible, PMP, SAN)– 4Fluoropolymers (4)Fluoropolymers: 4 × A, very good resistance (PTFE, FEP, PVDF, ECTFE/ETFE)A 4Elastomers (4)Elastomers: 2 × A, very good resistance (EPDM, NBR)A 2Elastomers: 1 × B, good resistance (Viton (FPM))B 1Elastomers: 1 × no data (Silicone)– 1Metals (3)Metals: 3 × A, very good resistance (SS 316, SS 304, Aluminium)A 3
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Number of materials in each family with each rating at 20 °C.

Effect of temperature, 20 °C to 50 °C

Ammonium Nitrate: Effect of temperature, 20 °C to 50 °CHDPE A → C; PVC Rigid A → C; Acetal (POM) B → D.ABCDHDPE: A at 20 °C, C at 50 °CHDPEPVC Rigid: A at 20 °C, C at 50 °CPVC RigidAcetal (POM): B at 20 °C, D at 50 °CAcetal (POM)
20 °C50 °C
Materials whose rating differs between 20 °C and 50 °C. Materials not shown keep their rating or have no 50 °C value.

Substance

CAS number
6484-52-2
Formula
(NH4)NO3
Hazard symbols in the source
O (oxidising) (pre-GHS European symbols; check the current safety data sheet)
Concentrations listed
10 %; saturated
Name in the source (German)
Ammoniumnitrat

Rating by concentration

Ammonium Nitrate: Rating by concentrationHDPE: 10 % A→C, saturated A→C. LDPE: 10 % –, saturated A. PP: 10 % A, saturated A. PVC Rigid: 10 % A→C, saturated A. PVC Flexible: 10 % –, saturated A. PMP: 10 % –, saturated A. Polystyrene: 10 % A, saturated A. SAN: 10 % –, saturated A. Polycarbonate: 10 % A*, saturated A. PETG: 10 % B*, saturated B*. Acetal (POM): 10 % B→D, saturated B→D. Nylon (PA): 10 % A, saturated A. Polysulfone: 10 % A, saturated A. PTFE: 10 % A, saturated A. FEP: 10 % A, saturated A. PVDF: 10 % A, saturated A. ECTFE/ETFE: 10 % A, saturated A. EPDM: 10 % A, saturated A. Viton (FPM): 10 % B, saturated B. NBR: 10 % A, saturated A. SS 316: 10 % A, saturated A. SS 304: 10 % A, saturated A. Aluminium: 10 % A, saturated B*.10 %saturatedTHERMOPLASTICSHDPEHDPE, 10 %: A at 20 °C, C at 50 °CA→CHDPE, saturated: A at 20 °C, C at 50 °CA→CLDPELDPE, 10 %: no data–LDPE, saturated: A at 20 °C, A at 50 °CAPPPP, 10 %: A at 20 °C, A at 50 °CAPP, saturated: A at 20 °C, A at 50 °CAPVC RigidPVC Rigid, 10 %: A at 20 °C, C at 50 °CA→CPVC Rigid, saturated: A at 20 °C, A at 50 °CAPVC FlexiblePVC Flexible, 10 %: no data–PVC Flexible, saturated: A at 20 °CAPMPPMP, 10 %: no data–PMP, saturated: A at 20 °C, A at 50 °CAPolystyrenePolystyrene, 10 %: A at 20 °C, A at 50 °CAPolystyrene, saturated: A at 20 °CASANSAN, 10 %: no data–SAN, saturated: A at 20 °C, A at 50 °CAPolycarbonatePolycarbonate, 10 %: A at 20 °C (estimate)A*Polycarbonate, saturated: A at 20 °CAPETGPETG, 10 %: B at 20 °C (estimate)B*PETG, saturated: B at 20 °C (estimate)B*Acetal (POM)Acetal (POM), 10 %: B at 20 °C, D at 50 °CB→DAcetal (POM), saturated: B at 20 °C, D at 50 °CB→DNylon (PA)Nylon (PA), 10 %: A at 20 °CANylon (PA), saturated: A at 20 °CAPolysulfonePolysulfone, 10 %: A at 20 °CAPolysulfone, saturated: A at 20 °CAFLUOROPOLYMERSPTFEPTFE, 10 %: A at 20 °C, A at 50 °CAPTFE, saturated: A at 20 °C, A at 50 °CAFEPFEP, 10 %: A at 20 °C, A at 50 °CAFEP, saturated: A at 20 °C, A at 50 °CAPVDFPVDF, 10 %: A at 20 °C, A at 50 °CAPVDF, saturated: A at 20 °C, A at 50 °CAECTFE/ETFEECTFE/ETFE, 10 %: A at 20 °C, A at 50 °CAECTFE/ETFE, saturated: A at 20 °C, A at 50 °CAELASTOMERSEPDMEPDM, 10 %: A at 20 °CAEPDM, saturated: A at 20 °CAViton (FPM)Viton (FPM), 10 %: B at 20 °C, B at 50 °CBViton (FPM), saturated: B at 20 °C, B at 50 °CBNBRNBR, 10 %: A at 20 °C, A at 50 °CANBR, saturated: A at 20 °C, A at 50 °CAMETALSSS 316SS 316, 10 %: A at 20 °C, A at 50 °CASS 316, saturated: A at 20 °C, A at 50 °CASS 304SS 304, 10 %: A at 20 °C, A at 50 °CASS 304, saturated: A at 20 °C, A at 50 °CAAluminiumAluminium, 10 %: A at 20 °C, A at 50 °CAAluminium, saturated: B at 20 °C (estimate)B*
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each cell shows the rating at 20 °C. Where the rating at 50 °C differs, it follows the arrow. * marks an estimate in the source.
Show as a table
Material10 %saturated
Thermoplastics
HDPEAA
LDPE–A
PPAA
PVC RigidAA
PVC Flexible–A
PMP–A
PolystyreneAA
SAN–A
PolycarbonateA*A
PETGB*B*
Acetal (POM)BB
Nylon (PA)AA
PolysulfoneAA
Fluoropolymers
PTFEAA
FEPAA
PVDFAA
ECTFE/ETFEAA
Elastomers
EPDMAA
Viton (FPM)BB
NBRAA
Silicone––
Metals
SS 316AA
SS 304AA
AluminiumAB*

* estimated rating, given in the source without a temperature

Resistance table: Ammonium Nitrate, 10 %

Material20 °C50 °CRemark
Thermoplastics
HDPEAC
PPAA
PVC RigidAC
PolystyreneAA
PolycarbonateA*–
PETGB*–
Acetal (POM)BD
Nylon (PA)A–
PolysulfoneA–
Fluoropolymers
PTFEAA
FEPAA
PVDFAA
ECTFE/ETFEAA
Elastomers
EPDMA–
Viton (FPM)BB
NBRAA
Metals
SS 316AA
SS 304AA
AluminiumAA

* estimated rating, given in the source without a temperature

Not rated in the source, so not in the table: LDPE, PVC Flexible, PMP, SAN, Silicone

Resistance table: Ammonium Nitrate, saturated

Material20 °C50 °CRemark
Thermoplastics
HDPEAC
LDPEAA
PPAA
PVC RigidAA
PVC FlexibleA–
PMPAA
PolystyreneA–
SANAA
PolycarbonateA–
PETGB*–
Acetal (POM)BD
Nylon (PA)A–
PolysulfoneA–
Fluoropolymers
PTFEAA
FEPAA
PVDFAA
ECTFE/ETFEAA
Elastomers
EPDMA–
Viton (FPM)BB
NBRAA
Metals
SS 316AA
SS 304AA
AluminiumB*–

* estimated rating, given in the source without a temperature

Not rated in the source, so not in the table: Silicone

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

Frequently Asked Questions

Which materials resist Ammonium Nitrate at high concentrations?

The materials with an A rating (resistant) for Ammonium Nitrate at 20 °C are: PTFE, HDPE, PP, PVDF, PVC Rigid, EPDM, NBR, SS 316. These can generally be used in direct contact.

Does temperature affect chemical resistance to Ammonium Nitrate?

Yes. 3 of 14 tested materials show a worse rating at 50 °C than at 20 °C for Ammonium Nitrate. Materials affected include: HDPE, PVC Rigid, Acetal (POM).

Is PTFE safe for Ammonium Nitrate?

PTFE is rated A for Ammonium Nitrate at 20 °C. A rating of A means resistant, B means limited resistance, C means partly resistant, and D means not resistant.

Does concentration affect chemical resistance to Ammonium Nitrate?

Yes. Ammonium Nitrate is tested at 2 concentrations (10 %, saturated). Some materials change their rating depending on the concentration.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.

Chemicals with a similar resistance profile

Same 20 °C rating on the share of materials shown.