Aluminium and Arsenic Acid: Chemical Resistance

Aluminium

Rating

Concentration20 °C50 °CRemark
aqueousDD
concentration not statedDD

Material comparison at 20 °C

Arsenic Acid: Material comparison at 20 °CAluminium: D (highlighted); ECTFE/ETFE: A; EPDM: A; FEP: A; HDPE: A; NBR: A.ECTFE/ETFE: AEPDM: AFEP: AHDPE: ANBR: APolycarbonate: APP: APolystyrene: APTFE: APVC Rigid: APVDF: ASS 304: ASS 316: AViton (FPM): BNylon (PA): CPVC Flexible: CAluminium: DAlAcetal (POM): DLDPE: –PETG: –PMP: –Polysulfone: –SAN: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Aluminium maintains a consistent rating of D across all 2 tested concentrations (aqueous) of Arsenic Acid at 20 °C. The fact that the rating does not change with concentration within the tested range simplifies material selection, though the boundary conditions beyond this range remain untested. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Arsenic Acid is commonly encountered in water treatment and laboratory work. Aluminium (Aluminium) is a metal typically used for vessels, heat exchangers, fittings and structural components. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.

Practical recommendation

Aluminium is not recommended for use with Arsenic Acid. The D rating indicates that the material will suffer rapid and severe degradation, which may include cracking, dissolution, severe swelling, or complete structural failure. Using this combination risks equipment damage, leaks, and potential safety incidents. Consider using HDPE, Polycarbonate, PP instead, which are rated A for this chemical and offer reliable long-term performance.

Did you know?

Temperature is often the deciding factor when selecting materials for Arsenic Acid: even materials rated A at 20 °C may lose performance at elevated temperatures.

Materials rated A or B at 20 °C

Based on the row for aqueous, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, Polycarbonate A, Polystyrene A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A, Viton (FPM) B, NBR A
Metals
SS 316 A, SS 304 A

About Aluminium

Aluminium relies on a thin oxide layer. Strong acids, strong alkalis and mercury compounds destroy that layer.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.