ChemicalResistance.org ← Search
HomeChemicalsAscorbic Acid › Nylon (PA)

Ascorbic Acid Resistance of Nylon (PA)

Is Nylon (PA) compatible with Ascorbic Acid? See the chemical resistance rating below.

Compatibility Rating

At 20°C (68°F)
B
Good
Good resistance - suitable for intermittent contact
At 50°C (122°F)
B
Good
Good resistance - suitable for intermittent contact

Comparison Table — All Materials for Ascorbic Acid

Material20°C50°C
HDPEAA
LDPEAA
PPAA
PTFEAA
PVDFAA
FEPAA
ECTFE/ETFEAA
EPDMAA
Viton (FPM)AA
NBRAA
SiliconeNRNR
SS 316AA
SS 304AA
AluminiumAA
PVC RigidNRNR
PVC FlexibleNRNR
PMPNRNR
PolystyreneNRNR
SANNRNR
PolycarbonateBB
PETGAA
Acetal (POM)BB
Nylon (PA)BB
PolysulfoneNRNR

A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data

🌡️ Temperature Note

Good resistance at both 20°C and 50°C. Maximum service temperature for this material is 100°C — above this, degradation risk increases significantly.

🔄 Better Alternative?

Consider: PVDF or PTFE. View all materials for Ascorbic Acid →

FAQ

Is Nylon (PA) resistant to Ascorbic Acid?

Nylon (PA) has Good (B) resistance to Ascorbic Acid at 20°C. Good resistance - suitable for intermittent contact.

Can I store Ascorbic Acid in Nylon (PA) containers?

Yes, Nylon (PA) is rated B (Good) for Ascorbic Acid.

All Materials for Ascorbic Acid All Chemicals for Nylon (PA)