ChemicalResistance
ChemicalResistance.org

Viton (FPM) and Butyric Acid: Chemical Resistance

Fluoroelastomer (FKM/FPM)

Rating

Concentration20 °C50 °CRemark
concentration not statedCD

Material comparison at 20 °C

Butyric Acid: Material comparison at 20 °CViton (FPM): C (highlighted); Aluminium: A; ECTFE/ETFE: A; FEP: A; PTFE: A; PVDF: A.Aluminium: AECTFE/ETFE: AFEP: APTFE: APVDF: ASS 304: ASS 316: APolysulfone: BPVC Rigid: BViton (FPM): CFPMHDPE: CNylon (PA): CEPDM: DLDPE: DNBR: DPolycarbonate: DPMP: DAcetal (POM): DPP: DPolystyrene: DPVC Flexible: DSAN: DPETG: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Viton (FPM) has limited resistance (C) to Butyric Acid at 20 °C. This indicates that the chemical has a noticeable effect on the material, which may include visible swelling, softening, or a measurable loss of tensile strength. Use is generally limited to short-term or intermittent contact where full structural integrity is not required. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Butyric Acid is commonly encountered in surface cleaning and metal finishing. Viton (FPM) (Fluoroelastomer (FKM/FPM)) is an elastomer typically used for seals, O-rings, hoses and flexible connections. Because Butyric Acid is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

Viton (FPM) has limited resistance to Butyric Acid and should only be used for short-term or intermittent contact at ambient temperature. The C rating means the material undergoes noticeable changes — swelling, loss of strength, or surface degradation — that make it unsuitable for permanent installations. For prolonged or continuous exposure, ECTFE/ETFE, FEP, PTFE offer significantly better resistance and are rated A.

Did you know?

When choosing between elastomers for Butyric Acid service, engineers consider not just the resistance rating but also factors such as permeation rate, creep resistance, and weldability.

Materials rated A or B at 20 °C

Thermoplastics
PVC Rigid B, Polysulfone B
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Metals
SS 316 A, SS 304 A, Aluminium A

About Viton (FPM)

Fluoroelastomer (Viton, FKM/FPM) resists fuels, oils and many acids. Ketones, esters, amines and hot water or steam attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.