ChemicalResistance
ChemicalResistance.org

Acetal (POM) and Calcium Sulfide: Chemical Resistance

Polyoxymethylene (acetal)

Rating

Concentration20 °C50 °CRemark
aqueousA*–
concentration not statedA*–

* estimated rating, given in the source without a temperature

Material comparison at 20 °C

Calcium Sulfide: Material comparison at 20 °CAcetal (POM): A (highlighted); Aluminium: A; EPDM: A; FEP: A; Viton (FPM): A; PP: A.Aluminium: AEPDM: AFEP: AViton (FPM): AAcetal (POM): APOMPP: APTFE: APVC Rigid: APVDF: ASS 304: ASS 316: ANylon (PA): BPolycarbonate: BLDPE: CNBR: CECTFE/ETFE: –HDPE: –PETG: –PMP: –Polystyrene: –Polysulfone: –PVC Flexible: –SAN: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Acetal (POM) shows excellent resistance to Calcium Sulfide across all 2 tested concentrations (aqueous) at 20 °C, making it a reliable choice for storage, transfer, and handling applications involving this chemical at any of the tested strengths. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Calcium Sulfide is commonly encountered in laboratory work and surface cleaning. Acetal (POM) (Polyoxymethylene (acetal)) is a thermoplastic typically used for tanks, piping, containers and liners. Because Calcium Sulfide is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

Acetal (POM) can be used with confidence for Calcium Sulfide containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. This holds true at both 20 °C and 50 °C, giving a good safety margin for typical process environments.

Did you know?

Chemical resistance testing according to DIN and ISO standards typically evaluates weight change, dimensional change, and retention of tensile strength after immersion.

Materials rated A or B at 20 °C

Based on the row for concentration not stated, 20 °C.

Thermoplastics
PP A, PVC Rigid A, Nylon (PA) B, Polycarbonate B
Fluoropolymers
PTFE A, PVDF A, FEP A
Elastomers
EPDM A, Viton (FPM) A
Metals
SS 316 A, SS 304 A, Aluminium A

About Acetal (POM)

Acetal (POM) resists many organic solvents and fuels. Strong acids and oxidising agents degrade it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.