Rating
| Concentration | 20 °C | 50 °C | Remark |
|---|---|---|---|
| concentration not stated | D* | – |
* estimated rating, given in the source without a temperature
Material comparison at 20 °C
Resistance overview
Viton (FPM) is not resistant (D) to Diethyl Ketone and should not be used in direct contact. The chemical is expected to cause rapid degradation, which can include dissolution, cracking, severe swelling, or complete structural failure of the material.
Application context
Diethyl Ketone is commonly encountered in de-icing and food processing. Viton (FPM) (Fluoroelastomer (FKM/FPM)) is an elastomer typically used for seals, O-rings, hoses and flexible connections. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.
Practical recommendation
Viton (FPM) is not recommended for use with Diethyl Ketone. The D rating indicates that the material will suffer rapid and severe degradation, which may include cracking, dissolution, severe swelling, or complete structural failure. Using this combination risks equipment damage, leaks, and potential safety incidents. Consider using Acetal (POM), FEP, PTFE instead, which are rated A for this chemical and offer reliable long-term performance.
Did you know?
In industrial practice, Viton (FPM) components exposed to Diethyl Ketone are typically inspected for swelling, discoloration, or loss of mechanical strength as early indicators of chemical attack.
Materials rated A or B at 20 °C
- Thermoplastics
- HDPE B, PP B, LDPE B, Acetal (POM) A, PMP B
- Fluoropolymers
- PTFE A, FEP A, ECTFE/ETFE B
- Metals
- SS 316 A, SS 304 A, Aluminium A
About Viton (FPM)
Fluoroelastomer (Viton, FKM/FPM) resists fuels, oils and many acids. Ketones, esters, amines and hot water or steam attack it.
Rating scale
- A very good resistance
- B good resistance
- C limited resistance
- D not resistant
- – no data
- K no general statement possible
A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.
About this data
The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.
A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.