Fluoroelastomer (FKM/FPM)

Rating

Concentration20 °C50 °CRemark
saturatedAA

Materials rated A or B at 20 °C

Based on the row for saturated, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, LDPE A, Polycarbonate A, PVC Flexible A, Polystyrene A, Polysulfone A, PMP A, SAN A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A, NBR A

About Viton (FPM)

Fluoroelastomer (Viton, FKM/FPM) resists fuels, oils and many acids. Ketones, esters, amines and hot water or steam attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.