Viton (FPM) and Lactic Acid: Chemical Resistance

Fluoroelastomer (FKM/FPM)

Rating

Concentration20 °C50 °CRemark
3 %AA
80 %AA
85 %AA

Material comparison at 20 °C

Lactic Acid: Material comparison at 20 °CViton (FPM): A (highlighted); Aluminium: A; ECTFE/ETFE: A; FEP: A; HDPE: A; LDPE: A.Aluminium: AECTFE/ETFE: AFEP: AViton (FPM): AFPMHDPE: ALDPE: ANBR: APolycarbonate: APMP: APP: APolysulfone: APTFE: APVDF: ASAN: ASS 304: ASS 316: APolystyrene: BPVC Rigid: BPVC Flexible: BEPDM: CNylon (PA): CAcetal (POM): CPETG: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Viton (FPM) shows excellent resistance to Lactic Acid across all 3 tested concentrations (3 %, 80 %, 85 %) at 20 °C, making it a reliable choice for storage, transfer, and handling applications involving this chemical at any of the tested strengths. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Lactic Acid is commonly encountered in water treatment and laboratory work. Viton (FPM) (Fluoroelastomer (FKM/FPM)) is an elastomer typically used for seals, O-rings, hoses and flexible connections. Because Lactic Acid is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

Viton (FPM) can be used with confidence for Lactic Acid containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. This holds true at both 20 °C and 50 °C, giving a good safety margin for typical process environments.

Did you know?

In industrial practice, Viton (FPM) components exposed to Lactic Acid are typically inspected for swelling, discoloration, or loss of mechanical strength as early indicators of chemical attack.

Materials rated A or B at 20 °C

Based on the row for 85 %, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid B, LDPE A, Polycarbonate A, PVC Flexible B, Polystyrene B, Polysulfone A, PMP A, SAN A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
NBR A
Metals
SS 316 A, SS 304 A, Aluminium A

About Viton (FPM)

Fluoroelastomer (Viton, FKM/FPM) resists fuels, oils and many acids. Ketones, esters, amines and hot water or steam attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.