Rating
| Concentration | 20 °C | 50 °C | Remark |
|---|---|---|---|
| concentration not stated | D | D |
Materials rated A or B at 20 °C
- Thermoplastics
- HDPE A, PP B, LDPE B, Nylon (PA) B, Acetal (POM) B
- Fluoropolymers
- PTFE A, PVDF B, FEP A, ECTFE/ETFE A
- Metals
- SS 316 A, SS 304 A, Aluminium A
About Viton (FPM)
Fluoroelastomer (Viton, FKM/FPM) resists fuels, oils and many acids. Ketones, esters, amines and hot water or steam attack it.
Rating scale
- A very good resistance
- B good resistance
- C limited resistance
- D not resistant
- – no data
- K no general statement possible
A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.
About this data
The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.
A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.