Viton (FPM) and Sodium Bicarbonate: Chemical Resistance

Fluoroelastomer (FKM/FPM)

Rating

Concentration20 °C50 °CRemark
aqueousAA

Material comparison at 20 °C

Sodium Bicarbonate: Material comparison at 20 °CViton (FPM): A (highlighted); Aluminium: A; ECTFE/ETFE: A; EPDM: A; FEP: A; HDPE: A.Aluminium: AECTFE/ETFE: AEPDM: AFEP: AViton (FPM): AFPMHDPE: ALDPE: ANBR: ANylon (PA): APolycarbonate: APETG: AAcetal (POM): APP: APTFE: APVDF: ASS 304: ASS 316: APMP: –Polystyrene: –Polysulfone: –PVC Rigid: –PVC Flexible: –SAN: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Viton (FPM) shows very good resistance (A) to Sodium Bicarbonate at aqueous at 20 °C, meaning the material remains essentially unaffected by this chemical under standard laboratory test conditions. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Sodium Bicarbonate is commonly encountered in de-icing and food processing. Viton (FPM) (Fluoroelastomer (FKM/FPM)) is an elastomer typically used for seals, O-rings, hoses and flexible connections. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.

Practical recommendation

Viton (FPM) can be used with confidence for Sodium Bicarbonate containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. This holds true at both 20 °C and 50 °C, giving a good safety margin for typical process environments.

Did you know?

The chemical resistance of Viton (FPM) depends not only on the chemical concentration but also on exposure time, mechanical stress, and the presence of other chemicals in the mixture.

Materials rated A or B at 20 °C

Based on the row for aqueous, 20 °C.

Thermoplastics
HDPE A, PP A, LDPE A, Nylon (PA) A, Acetal (POM) A, Polycarbonate A, PETG A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A, NBR A
Metals
SS 316 A, SS 304 A, Aluminium A

About Viton (FPM)

Fluoroelastomer (Viton, FKM/FPM) resists fuels, oils and many acids. Ketones, esters, amines and hot water or steam attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.