ChemicalResistance ChemicalResistance.org ← Search
Home Chemicals Sodium Nitrate Nylon (PA)

Sodium Nitrate Resistance of Nylon (PA)

Is Nylon (PA) compatible with Sodium Nitrate?

Compatibility Rating

At 20°C
A
Excellent
Excellent resistance - recommended for continuous use
At 50°C
NR
No Data
No data available

Comparison Table — All Materials for Sodium Nitrate

Material20°C50°C
HDPEAA
LDPEAA
PPAA
PTFEAA
PVDFAA
FEPAA
ECTFE/ETFEAA
EPDMANR
Viton (FPM)AA
NBRANR
SiliconeNRNR
SS 316AA
SS 304AA
AluminiumAA
PVC RigidNRNR
PVC FlexibleNRNR
PMPNRNR
PolystyreneNRNR
SANNRNR
PolycarbonateANR
PETGANR
Acetal (POM)AA
Nylon (PA)ANR
PolysulfoneNRNR

A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data

🌡️ Temperature Note

Good resistance at both 20°C and 50°C. Maximum service temperature for this material is 100°C — above this, degradation risk increases significantly.

🔄 Better Alternative?

Consider: PVDF or PTFE. View all materials for Sodium Nitrate →

FAQ

Is Nylon (PA) resistant to Sodium Nitrate?

Nylon (PA) has Excellent (A) resistance to Sodium Nitrate at 20°C.

Can I store Sodium Nitrate in Nylon (PA)?

Yes, Nylon (PA) is rated A for Sodium Nitrate.

All Materials for Sodium Nitrate All Chemicals for Nylon (PA)