Concentration20 °C50 °CRemark
10 %AA
aqueousAA

Material comparison at 20 °C

Zinc Chloride: Material comparison at 20 °CViton (FPM): A (highlighted); ECTFE/ETFE: A; EPDM: A; FEP: A; HDPE: A; LDPE: A.ECTFE/ETFE: AEPDM: AFEP: AViton (FPM): AFPMHDPE: ALDPE: ANBR: APolycarbonate: APMP: APP: APolystyrene: APTFE: APVC Rigid: APVC Flexible: APVDF: ASAN: ASS 304: ASS 316: AAcetal (POM): BAluminium: CNylon (PA): CPETG: –Polysulfone: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Viton (FPM) shows excellent resistance to Zinc Chloride across all 2 tested concentrations (10 %, aqueous) at 20 °C, making it a reliable choice for storage, transfer, and handling applications involving this chemical at any of the tested strengths. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Zinc Chloride is commonly encountered in water disinfection and waste treatment. Viton (FPM) (Fluoroelastomer (FKM/FPM)) is an elastomer typically used for seals, O-rings, hoses and flexible connections. Because Zinc Chloride is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

Viton (FPM) can be used with confidence for Zinc Chloride containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. This holds true at both 20 °C and 50 °C, giving a good safety margin for typical process environments.

Did you know?

The chemical resistance of Viton (FPM) depends not only on the chemical concentration but also on exposure time, mechanical stress, and the presence of other chemicals in the mixture.

Materials rated A or B at 20 °C

Based on the row for 10 %, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, LDPE A, Acetal (POM) B, Polycarbonate A, PVC Flexible A, Polystyrene A, PMP A, SAN A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A, NBR A
Metals
SS 316 A, SS 304 A

About Viton (FPM)

Fluoroelastomer (Viton, FKM/FPM) resists fuels, oils and many acids. Ketones, esters, amines and hot water or steam attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.