Polyoxymethylene (acetal)

Rating

Concentration20 °C50 °CRemark
10 %AB
30 %AB
40 %AB

Material comparison at 20 °C

Formaldehyde Solution: Material comparison at 20 °CAcetal (POM): A (highlighted); Aluminium: A; ECTFE/ETFE: A; EPDM: A; FEP: A; HDPE: A.Aluminium: AECTFE/ETFE: AEPDM: AFEP: AHDPE: ANylon (PA): APolycarbonate: APETG: APMP: AAcetal (POM): APOMPP: APTFE: APVDF: ASS 304: ASS 316: ALDPE: BPolysulfone: BPVC Rigid: BViton (FPM): CNBR: CPVC Flexible: CPolystyrene: DSAN: –Silicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Acetal (POM) shows excellent resistance to Formaldehyde Solution across all 3 tested concentrations (10 %, 30 %, 40 %) at 20 °C, making it a reliable choice for storage, transfer, and handling applications involving this chemical at any of the tested strengths. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Formaldehyde Solution is commonly encountered in electroplating and chemical storage. Acetal (POM) (Polyoxymethylene (acetal)) is a thermoplastic typically used for tanks, piping, containers and liners. The compatibility between these two is therefore an important consideration for engineers and procurement teams selecting containment, transfer, or processing equipment.

Practical recommendation

Acetal (POM) can be used with confidence for Formaldehyde Solution containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. At elevated temperatures (50 °C), some reduction in resistance occurs, so periodic inspection is advisable for heated applications. Always verify performance under actual operating conditions before committing to a design.

Did you know?

Chemical resistance testing according to DIN and ISO standards typically evaluates weight change, dimensional change, and retention of tensile strength after immersion.

Materials rated A or B at 20 °C

Based on the row for 40 %, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid B, LDPE B, Nylon (PA) A, Polycarbonate A, Polysulfone B, PETG A, PMP A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A
Metals
SS 316 A, SS 304 A, Aluminium A

About Acetal (POM)

Acetal (POM) resists many organic solvents and fuels. Strong acids and oxidising agents degrade it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.