ChemicalResistance
ChemicalResistance.org

Viton (FPM) and Perchloric Acid: Chemical Resistance

Fluoroelastomer (FKM/FPM)

Rating

Concentration20 °C50 °CRemark
20 %AA
70 %AA

Material comparison at 20 °C

Perchloric Acid: Material comparison at 20 °CViton (FPM): A (highlighted); ECTFE/ETFE: A; FEP: A; PTFE: A; PVDF: A; HDPE: B.ECTFE/ETFE: AFEP: AViton (FPM): AFPMPTFE: APVDF: AHDPE: BPMP: BPolystyrene: BEPDM: CLDPE: CPVC Rigid: CAluminium: DNBR: DNylon (PA): DPolycarbonate: DPETG: DAcetal (POM): DPP: DPolysulfone: DPVC Flexible: DSAN: –Silicone: –SS 304: –SS 316: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Viton (FPM) shows excellent resistance to Perchloric Acid across all 2 tested concentrations (20 %, 70 %) at 20 °C, making it a reliable choice for storage, transfer, and handling applications involving this chemical at any of the tested strengths. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Perchloric Acid is commonly encountered in surface cleaning and chemical processing. Viton (FPM) (Fluoroelastomer (FKM/FPM)) is an elastomer typically used for seals, O-rings, hoses and flexible connections. Because Perchloric Acid is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

Viton (FPM) can be used with confidence for Perchloric Acid containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. This holds true at both 20 °C and 50 °C, giving a good safety margin for typical process environments.

Did you know?

The chemical resistance of Viton (FPM) depends not only on the chemical concentration but also on exposure time, mechanical stress, and the presence of other chemicals in the mixture.

Materials rated A or B at 20 °C

Based on the row for 70 %, 20 °C.

Thermoplastics
HDPE B, Polystyrene B, PMP B
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A

About Viton (FPM)

Fluoroelastomer (Viton, FKM/FPM) resists fuels, oils and many acids. Ketones, esters, amines and hot water or steam attack it.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.