ChemicalResistance ChemicalResistance.org ← Search
Home Chemicals Tartaric Acid Stainless Steel 304

Tartaric Acid Resistance of Stainless Steel 304

Is Stainless Steel 304 compatible with Tartaric Acid?

Compatibility Rating

At 20°C
A
Excellent
Excellent resistance - recommended for continuous use
At 50°C
C
Fair
Limited resistance - short-term exposure only

Why is SS 304 resistant to Tartaric Acid?

SS 304 shows excellent resistance to Tartaric Acid due to its chromium content (18%) forming a passive oxide layer resistant to many corrosive environments.

⚠️ When NOT to use SS 304

Avoid using Stainless Steel 304 with chloride-rich environments (seawater, HCl) which cause pitting corrosion. Use 316 grade for chloride exposure.

Comparison Table — All Materials for Tartaric Acid

Material20°C50°C
HDPEAA
LDPEAA
PPAA
PTFEAA
PVDFAA
FEPAA
ECTFE/ETFEAA
EPDMCNR
Viton (FPM)AA
NBRAA
SiliconeNRNR
SS 316AB
SS 304AC
AluminiumDD
PVC RigidAB
PVC FlexibleAC
PMPAA
PolystyreneBB
SANAA
PolycarbonateAB
PETGNRNR
Acetal (POM)CC
Nylon (PA)DD
PolysulfoneAA

A=Excellent · B=Good · C=Fair · D=Poor · NR=No Data

🌡️ Temperature Note

Performance degrades significantly at higher temperatures — rated Excellent at 20°C but only Fair at 50°C. For elevated temperatures, consider a more resistant material. Max service temp: 800°C.

🔄 Better Alternative?

Consider: SS 316 for chloride environments. View all materials for Tartaric Acid →

FAQ

Is Stainless Steel 304 resistant to Tartaric Acid?

Stainless Steel 304 has Excellent (A) resistance to Tartaric Acid at 20°C.

Can I store Tartaric Acid in Stainless Steel 304?

Yes, Stainless Steel 304 is rated A for Tartaric Acid.

All Materials for Tartaric Acid All Chemicals for Stainless Steel 304