ChemicalResistance
ChemicalResistance.org

ECTFE/ETFE and Silver Nitrate: Chemical Resistance

Ethylene chlorotrifluoroethylene / ethylene tetrafluoroethylene

Rating

Concentration20 °C50 °CRemark
aqueous––
concentration not statedAA

Material comparison at 20 °C

Silver Nitrate: Material comparison at 20 °CECTFE/ETFE: A (highlighted); EPDM: A; FEP: A; Viton (FPM): A; HDPE: A; LDPE: A.ECTFE/ETFE: AECTFEEPDM: AFEP: AViton (FPM): AHDPE: ALDPE: ANylon (PA): APolycarbonate: APMP: AAcetal (POM): APP: APolysulfone: APTFE: APVC Rigid: APVC Flexible: APVDF: ASAN: ASS 304: ASS 316: APETG: BPolystyrene: BNBR: CAluminium: DSilicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

ECTFE/ETFE shows very good resistance (A) to Silver Nitrate at 20 °C, meaning the material remains essentially unaffected by this chemical under standard laboratory test conditions. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Silver Nitrate is commonly encountered in de-icing and chemical storage. ECTFE/ETFE (Ethylene chlorotrifluoroethylene / ethylene tetrafluoroethylene) is a fluoropolymer typically used for seals, gaskets, valve seats and lined equipment. Because Silver Nitrate is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

ECTFE/ETFE can be used with confidence for Silver Nitrate containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. This holds true at both 20 °C and 50 °C, giving a good safety margin for typical process environments.

Did you know?

In industrial practice, ECTFE/ETFE components exposed to Silver Nitrate are typically inspected for swelling, discoloration, or loss of mechanical strength as early indicators of chemical attack.

Materials rated A or B at 20 °C

Based on the row for concentration not stated, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, LDPE A, Nylon (PA) A, Acetal (POM) A, Polycarbonate A, PVC Flexible A, Polystyrene B, Polysulfone A, PETG B, PMP A, SAN A
Fluoropolymers
PTFE A, PVDF A, FEP A
Elastomers
EPDM A, Viton (FPM) A
Metals
SS 316 A, SS 304 A

About ECTFE/ETFE

ECTFE and ETFE are tough fluoropolymers with broad resistance. Hot amines and some chlorinated solvents at elevated temperature are their main limits.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.