Polycarbonate and Silver Nitrate: Chemical Resistance

Polycarbonate

Rating

Concentration20 °C50 °CRemark
aqueousAA
concentration not statedAA

Material comparison at 20 °C

Silver Nitrate: Material comparison at 20 °CPolycarbonate: A (highlighted); ECTFE/ETFE: A; EPDM: A; FEP: A; Viton (FPM): A; HDPE: A.ECTFE/ETFE: AEPDM: AFEP: AViton (FPM): AHDPE: ALDPE: ANylon (PA): APolycarbonate: APCPMP: AAcetal (POM): APP: APolysulfone: APTFE: APVC Rigid: APVC Flexible: APVDF: ASAN: ASS 304: ASS 316: APETG: BPolystyrene: BNBR: CAluminium: DSilicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

Polycarbonate shows excellent resistance to Silver Nitrate across all 2 tested concentrations (aqueous) at 20 °C, making it a reliable choice for storage, transfer, and handling applications involving this chemical at any of the tested strengths. The rating remains stable between 20 °C and 50 °C, which means this material can also handle moderately elevated process temperatures without additional risk.

Application context

Silver Nitrate is commonly encountered in electroplating and food processing. Polycarbonate (Polycarbonate) is a thermoplastic typically used for tanks, piping, containers and liners. Because Silver Nitrate is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

Polycarbonate can be used with confidence for Silver Nitrate containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. This holds true at both 20 °C and 50 °C, giving a good safety margin for typical process environments.

Did you know?

In industrial practice, Polycarbonate components exposed to Silver Nitrate are typically inspected for swelling, discoloration, or loss of mechanical strength as early indicators of chemical attack.

Materials rated A or B at 20 °C

Based on the row for concentration not stated, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, LDPE A, Nylon (PA) A, Acetal (POM) A, PVC Flexible A, Polystyrene B, Polysulfone A, PETG B, PMP A, SAN A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A, Viton (FPM) A
Metals
SS 316 A, SS 304 A

About Polycarbonate

Polycarbonate is attacked by alkalis, amines, ketones, esters and many organic solvents, and it stress-cracks under load in contact with them.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.