Flexible (plasticised) polyvinyl chloride

Rating

Concentration20 °C50 °CRemark
aqueous––
concentration not statedAC

Material comparison at 20 °C

Silver Nitrate: Material comparison at 20 °CPVC Flexible: A (highlighted); ECTFE/ETFE: A; EPDM: A; FEP: A; Viton (FPM): A; HDPE: A.ECTFE/ETFE: AEPDM: AFEP: AViton (FPM): AHDPE: ALDPE: ANylon (PA): APolycarbonate: APMP: AAcetal (POM): APP: APolysulfone: APTFE: APVC Rigid: APVC Flexible: APVC-PPVDF: ASAN: ASS 304: ASS 316: APETG: BPolystyrene: BNBR: CAluminium: DSilicone: –
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Each bar is one material. Taller bars indicate better resistance. The highlighted bar is the current material.

Resistance overview

PVC Flexible shows very good resistance (A) to Silver Nitrate at 20 °C, meaning the material remains essentially unaffected by this chemical under standard laboratory test conditions. However, at 50 °C the resistance rating drops, indicating that temperature must be factored into the design. For heated applications, additional testing under actual service conditions is strongly recommended.

Application context

Silver Nitrate is commonly encountered in water treatment and de-icing. PVC Flexible (Flexible (plasticised) polyvinyl chloride) is a thermoplastic typically used for tanks, piping, containers and liners. Because Silver Nitrate is classified as corrosive, the choice of containment material is especially critical to prevent leaks, equipment damage, and safety hazards.

Practical recommendation

PVC Flexible can be used with confidence for Silver Nitrate containment and handling. The A rating indicates that the material shows no significant change in weight, dimensions, or mechanical properties after prolonged contact under test conditions. At elevated temperatures (50 °C), some reduction in resistance occurs, so periodic inspection is advisable for heated applications. Always verify performance under actual operating conditions before committing to a design.

Did you know?

The ratings shown here apply to pure Silver Nitrate in contact with the base thermoplastic. In real-world applications, additives, pigments, and fillers in the material can shift resistance in either direction.

Materials rated A or B at 20 °C

Based on the row for concentration not stated, 20 °C.

Thermoplastics
HDPE A, PP A, PVC Rigid A, LDPE A, Nylon (PA) A, Acetal (POM) A, Polycarbonate A, Polystyrene B, Polysulfone A, PETG B, PMP A, SAN A
Fluoropolymers
PTFE A, PVDF A, FEP A, ECTFE/ETFE A
Elastomers
EPDM A, Viton (FPM) A
Metals
SS 316 A, SS 304 A

About PVC Flexible

Flexible PVC shares the solvent weaknesses of rigid PVC, and any liquid that extracts the plasticiser also hardens it. It is generally less resistant than rigid PVC.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.