ChemicalResistance
ChemicalResistance.org

Nylon (PA) vs Silicone: Chemical Resistance Compared

Of 22 source rows rated for both materials at 20 °C, 22 (100 %) have the same rating. Nylon (PA) is rated better in 0 rows and Silicone in 0. A row is one chemical at one concentration.

Summary

Silicone is rated better with
Salts and salt solutions (+22 points)

Points are the difference in the share of rows rated A or B.

The two materials

Nylon (PA)

Polyamide (nylon)

Polyamide (nylon) resists fuels, oils and many solvents. Mineral acids, even dilute, and strong oxidisers attack it, and it absorbs water.

Rated rows: 945. A 44 %, B 21 %, C 17 %, D 18 %

All chemicals for Nylon (PA)

Silicone

Silicone rubber

Silicone rubber keeps its flexibility over a wide temperature range. Concentrated acids and alkalis and hydrocarbon solvents attack or swell it.

Rated rows: 23. A 96 %, B 0 %, C 0 %, D 4 %

All chemicals for Silicone

Share of rows rated A or B, by chemical class

Nylon (PA), Silicone: Share of rows rated A or B, by chemical classSalts and salt solutions: Nylon (PA) 78 %, Silicone 100 %.Salts and salt solutionsSalts and salt solutions, Nylon (PA): 78 % (194)78 %Salts and salt solutions, Silicone: 100 % (9)100 %
Nylon (PA)Silicone
Rating at 20 °C. Only classes with at least 8 rated rows for both materials are shown.

How often the two ratings agree

Nylon (PA), Silicone: How often the two ratings agreeNylon (PA) A, Silicone A: 21; Nylon (PA) D, Silicone D: 1.SiliconeABCDNylon (PA)ANylon (PA) A, Silicone A: 2121Nylon (PA) A, Silicone B: 00Nylon (PA) A, Silicone C: 00Nylon (PA) A, Silicone D: 00BNylon (PA) B, Silicone A: 00Nylon (PA) B, Silicone B: 00Nylon (PA) B, Silicone C: 00Nylon (PA) B, Silicone D: 00CNylon (PA) C, Silicone A: 00Nylon (PA) C, Silicone B: 00Nylon (PA) C, Silicone C: 00Nylon (PA) C, Silicone D: 00DNylon (PA) D, Silicone A: 00Nylon (PA) D, Silicone B: 00Nylon (PA) D, Silicone C: 00Nylon (PA) D, Silicone D: 11
Number of source rows for each pair of ratings at 20 °C. Outlined cells are rows where both materials have the same rating.

Chemical classes were assigned by this site, not by the source. Mixtures and trade products without a clear class are not counted.

By chemical class

Chemical classNylon (PA): rated A or BSilicone: rated A or B
Mineral acids5 % (63 rows)–
Organic acids25 % (63 rows)–
Alkalis91 % (22 rows)–
Salts and salt solutions78 % (194 rows)100 % (9 rows)
Oxidising agents and halogens26 % (62 rows)–
Alcohols and glycols67 % (58 rows)–
Phenols8 % (13 rows)–
Ketones and aldehydes53 % (32 rows)–
Esters and ethers80 % (65 rows)–
Amines and nitrogen compounds50 % (34 rows)–
Aromatic hydrocarbons100 % (14 rows)–
Fuels, mineral oils and aliphatic hydrocarbons97 % (73 rows)–
Vegetable and animal oils, fats, essential oils98 % (46 rows)–
Halogenated hydrocarbons63 % (70 rows)–
Foods and beverages98 % (46 rows)–

Where the ratings differ most

No row has ratings more than one grade apart.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

More comparisons

Frequently Asked Questions

Is Nylon (PA) or Silicone more chemical-resistant?

Of 22 chemicals rated for both materials at 20 °C, Nylon (PA) and Silicone share the same rating in 22 rows (100 %). Nylon (PA) is rated better in 0 rows and Silicone in 0 rows.

How do Nylon (PA) and Silicone compare for chemical resistance?

Based on 22 chemicals tested for both: Nylon (PA) is rated better with –. Silicone is rated better with Salts and salt solutions. They perform similarly with –.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.