PP vs Silicone: Chemical Resistance Compared

Of 22 source rows rated for both materials at 20 °C, 22 (100 %) have the same rating. PP is rated better in 0 rows and Silicone in 0. A row is one chemical at one concentration.

Summary

Within 10 points of each other
Salts and salt solutions

Points are the difference in the share of rows rated A or B.

The two materials

PP

Polypropylene

Polypropylene resists most acids, alkalis and salt solutions. Concentrated oxidising acids, chlorinated solvents and aromatic hydrocarbons attack it, and it turns brittle below about 0 °C.

Rated rows: 978. A 66 %, B 11 %, C 15 %, D 8 %

All chemicals for PP

Silicone

Silicone rubber

Silicone rubber keeps its flexibility over a wide temperature range. Concentrated acids and alkalis and hydrocarbon solvents attack or swell it.

Rated rows: 23. A 96 %, B 0 %, C 0 %, D 4 %

All chemicals for Silicone

Share of rows rated A or B, by chemical class

PP, Silicone: Share of rows rated A or B, by chemical classSalts and salt solutions: PP 99 %, Silicone 100 %.Salts and salt solutionsSalts and salt solutions, PP: 99 % (198)99 %Salts and salt solutions, Silicone: 100 % (9)100 %
PPSilicone
Rating at 20 °C. Only classes with at least 8 rated rows for both materials are shown.

How often the two ratings agree

PP, Silicone: How often the two ratings agreePP A, Silicone A: 21; PP D, Silicone D: 1.SiliconeABCDPPAPP A, Silicone A: 2121PP A, Silicone B: 00PP A, Silicone C: 00PP A, Silicone D: 00BPP B, Silicone A: 00PP B, Silicone B: 00PP B, Silicone C: 00PP B, Silicone D: 00CPP C, Silicone A: 00PP C, Silicone B: 00PP C, Silicone C: 00PP C, Silicone D: 00DPP D, Silicone A: 00PP D, Silicone B: 00PP D, Silicone C: 00PP D, Silicone D: 11
Number of source rows for each pair of ratings at 20 °C. Outlined cells are rows where both materials have the same rating.

Chemical classes were assigned by this site, not by the source. Mixtures and trade products without a clear class are not counted.

By chemical class

Chemical classPP: rated A or BSilicone: rated A or B
Mineral acids70 % (63 rows)–
Organic acids97 % (64 rows)–
Alkalis100 % (22 rows)–
Salts and salt solutions99 % (198 rows)100 % (9 rows)
Oxidising agents and halogens72 % (61 rows)–
Alcohols and glycols93 % (59 rows)–
Phenols79 % (14 rows)–
Ketones and aldehydes69 % (35 rows)–
Esters and ethers63 % (71 rows)–
Amines and nitrogen compounds79 % (39 rows)–
Aromatic hydrocarbons14 % (14 rows)–
Fuels, mineral oils and aliphatic hydrocarbons63 % (78 rows)–
Vegetable and animal oils, fats, essential oils75 % (48 rows)–
Halogenated hydrocarbons4 % (70 rows)–
Foods and beverages100 % (46 rows)–

Where the ratings differ most

No row has ratings more than one grade apart.

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

More comparisons

Frequently Asked Questions

Is PP or Silicone more chemical-resistant?

Of 22 chemicals rated for both materials at 20 °C, PP and Silicone share the same rating in 22 rows (100 %). PP is rated better in 0 rows and Silicone in 0 rows.

How do PP and Silicone compare for chemical resistance?

Based on 22 chemicals tested for both: PP is rated better with –. Silicone is rated better with –. They perform similarly with Salts and salt solutions.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.