Resistance ratings for 24 plastics, elastomers and metals at 20 °C and 50 °C.

At a glance

Based on the row for any concentration, 20 °C.

Rated A, very good resistance
PTFE, HDPE, PP, PVDF, PVC Rigid, EPDM, Viton (FPM), NBR, SS 316, SS 304, Aluminium, LDPE, FEP, ECTFE/ETFE, Nylon (PA), Acetal (POM), Polycarbonate, Silicone, PVC Flexible, Polystyrene, Polysulfone, PETG, PMP, SAN (24)
Rated B, good resistance
none (0)
Rated C, limited resistance
none (0)
Rated D, not resistant
none (0)

Based on the row for any concentration, 20 °C.

Rating profile by material family

Glucose: Rating profile by material familyThermoplastics: 13 A. Fluoropolymers: 4 A. Elastomers: 4 A. Metals: 3 A.Thermoplastics (13)Thermoplastics: 13 × A, very good resistance (HDPE, LDPE, PP, PVC Rigid, PVC Flexible, PMP, Polystyrene, SAN, Polycarbonate, PETG, Acetal (POM), Nylon (PA), Polysulfone)A 13Fluoropolymers (4)Fluoropolymers: 4 × A, very good resistance (PTFE, FEP, PVDF, ECTFE/ETFE)A 4Elastomers (4)Elastomers: 4 × A, very good resistance (EPDM, Viton (FPM), NBR, Silicone)A 4Metals (3)Metals: 3 × A, very good resistance (SS 316, SS 304, Aluminium)A 3
A very good resistanceB good resistanceC limited resistanceD not resistantno data
Number of materials in each family with each rating at 20 °C.

Effect of temperature, 20 °C to 50 °C

No material with a rating at both temperatures changes grade between 20 °C and 50 °C.

Substance

CAS number
50-99-7
Formula
C6H12O6
Concentrations listed
any concentration
Also listed as
Dextrose (Glucose)
Name in the source (German)
Glucose

Resistance table: Glucose, any concentration

Material20 °C50 °CRemark
Thermoplastics
HDPEAA
LDPEAA
PPAA
PVC RigidAA
PVC FlexibleAA
PMPAA
PolystyreneAA
SANAA
PolycarbonateAA
PETGAA
Acetal (POM)AA
Nylon (PA)AA
PolysulfoneAA
Fluoropolymers
PTFEAA
FEPAA
PVDFAA
ECTFE/ETFEAA
Elastomers
EPDMAA
Viton (FPM)AA
NBRAA
SiliconeAA
Metals
SS 316AA
SS 304AA
AluminiumAA

Rating scale

A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.

About this data

The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.

A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.

Chemicals with a similar resistance profile

Same 20 °C rating on the share of materials shown.