At a glance
Based on the row for saturated, 20 °C.
- Rated A, very good resistance
- PTFE, HDPE, PP, PVDF, PVC Rigid, EPDM, Viton (FPM), SS 316, SS 304, Aluminium, LDPE, FEP, Nylon (PA), Acetal (POM), PVC Flexible, Polystyrene, PETG, PMP, SAN (19)
- Rated B, good resistance
- NBR, Polycarbonate (2)
- Rated C, limited resistance
- none (0)
- Rated D, not resistant
- none (0)
- No data in the source
- ECTFE/ETFE, Silicone, Polysulfone
- Rated lower at 50 °C than at 20 °C
- NBR (B → C)
- Rating changes with concentration (20 °C)
- NBR: A (aqueous), B (saturated)
Based on the row for saturated, 20 °C.
Rating profile by material family
Effect of temperature, 20 °C to 50 °C
Substance
- CAS number
- 7632-00-0
- Formula
- NaNO2
- Hazard symbols in the source
- O (oxidising), T (toxic) (pre-GHS European symbols; check the current safety data sheet)
- Concentrations listed
- aqueous; saturated
- Name in the source (German)
- Natriumnitrit
Rating by concentration
Show as a table
| Material | aqueous | saturated |
|---|---|---|
| Thermoplastics | ||
| HDPE | A | A |
| LDPE | A | A |
| PP | A | A |
| PVC Rigid | – | A |
| PVC Flexible | – | A |
| PMP | – | A |
| Polystyrene | – | A |
| SAN | – | A |
| Polycarbonate | B* | B* |
| PETG | A | A* |
| Acetal (POM) | A | A |
| Nylon (PA) | A | A |
| Polysulfone | – | – |
| Fluoropolymers | ||
| PTFE | A | A |
| FEP | A* | A* |
| PVDF | A | A |
| ECTFE/ETFE | – | – |
| Elastomers | ||
| EPDM | A | A |
| Viton (FPM) | A | A |
| NBR | A | B |
| Silicone | – | – |
| Metals | ||
| SS 316 | A | A |
| SS 304 | A | A |
| Aluminium | A | A |
* estimated rating, given in the source without a temperature
Resistance table: Sodium Nitrite, aqueous
| Material | 20 °C | 50 °C | Remark |
|---|---|---|---|
| Thermoplastics | |||
| HDPE | A | A | |
| LDPE | A | A | |
| PP | A | A | |
| Polycarbonate | B* | – | |
| PETG | A | – | |
| Acetal (POM) | A | A | |
| Nylon (PA) | A | – | |
| Fluoropolymers | |||
| PTFE | A | A | |
| FEP | A* | – | |
| PVDF | A | A | |
| Elastomers | |||
| EPDM | A | – | |
| Viton (FPM) | A | A | |
| NBR | A | – | |
| Metals | |||
| SS 316 | A | A | |
| SS 304 | A | A | |
| Aluminium | A | – | |
* estimated rating, given in the source without a temperature
Not rated in the source, so not in the table: PVC Rigid, PVC Flexible, PMP, Polystyrene, SAN, Polysulfone, ECTFE/ETFE, Silicone
Resistance table: Sodium Nitrite, saturated
| Material | 20 °C | 50 °C | Remark |
|---|---|---|---|
| Thermoplastics | |||
| HDPE | A | A | |
| LDPE | A | A | |
| PP | A | A | |
| PVC Rigid | A | – | |
| PVC Flexible | A | – | |
| PMP | A | – | |
| Polystyrene | A | A | |
| SAN | A | A | |
| Polycarbonate | B* | – | |
| PETG | A* | – | |
| Acetal (POM) | A | A | |
| Nylon (PA) | A | – | |
| Fluoropolymers | |||
| PTFE | A | A | |
| FEP | A* | – | |
| PVDF | A | A | |
| Elastomers | |||
| EPDM | A | – | |
| Viton (FPM) | A | A | |
| NBR | B | C | |
| Metals | |||
| SS 316 | A | A | |
| SS 304 | A | A | |
| Aluminium | A | – | |
* estimated rating, given in the source without a temperature
Not rated in the source, so not in the table: Polysulfone, ECTFE/ETFE, Silicone
Rating scale
- A very good resistance
- B good resistance
- C limited resistance
- D not resistant
- – no data
- K no general statement possible
A rating marked * is an estimate in the source, not a test result. An estimate is given as one value without a temperature.
Frequently Asked Questions
Which materials resist Sodium Nitrite at high concentrations?
The materials with an A rating (resistant) for Sodium Nitrite at 20 °C are: PTFE, HDPE, PP, PVDF, PVC Rigid, EPDM, Viton (FPM), SS 316. These can generally be used in direct contact.
Does temperature affect chemical resistance to Sodium Nitrite?
Yes. 1 of 12 tested materials show a worse rating at 50 °C than at 20 °C for Sodium Nitrite. Materials affected include: NBR.
Is PTFE safe for Sodium Nitrite?
PTFE is rated A for Sodium Nitrite at 20 °C. A rating of A means resistant, B means limited resistance, C means partly resistant, and D means not resistant.
Does concentration affect chemical resistance to Sodium Nitrite?
Yes. Sodium Nitrite is tested at 2 concentrations (aqueous, saturated). Some materials change their rating depending on the concentration.
About this data
The ratings come from the chemical resistance list published by Bürkle GmbH, which compiled them from raw-material manufacturers’ data. They describe laboratory tests on the raw material at 20 °C and 50 °C.
A finished part also sees pressure, mechanical stress, welds and mixtures that a laboratory test does not. Treat the rating as a first filter and test under your own conditions before relying on it.
Chemicals with a similar resistance profile